Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
SABIC MG200024 Linear Low Density Polyethylene for Compounding Product Description: MG200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding. It is in the powder form designed to give g.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Europe-Africa-Middle East) CYCOLAC FR15U is a flame retardant ABS with good processability and good indoor UV properties. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Vicat Softening Point | >= 92.0 °C | >= 198 °F | ASTM D1525 |
NIZHNEKAMSKNEFTEKHIM 525 General Purpose Polystyrene Grade 525 is a crystal polystyrene for both injection molding and cap layer co-extrusion. Injection molding applications such as medical and laboratory parts, tumblers, and jewel boxes demonstrate t.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total Lacqrene® 1240 Crystal Polystyrene
(discontinued **) LACQRENE® 1240 is a high molecular weight crystal polystyrene, used in the dilution of high impact grades of polystyrene such as LACQRENE® 7240 or clear impact polystyrene such as Finaclear 520. .. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Ineos Nova 3500 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Suitable for difficult to fill and thin wall molding, USP Class VIApplications: Cosmetic and medical packaging, Housewares, Consumer Electronic packaging, ToysExposure to gamma .. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
ExxonMobil LD 051.LJ Molding, Extrusion and Compounding Resin
(discontinued **) LD 051.LJ resin is used in Blow molded, squeeze bottles, Pail lids, Closures, and Extruded profiles.Information provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Huntsman PE1023 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good draw down characteristics.Applications: Film extrusion: drum liners, hardware packaging, and refuse bags.FDA Notes: Conforms to FDA regulation 21 CFR 17.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | |
Ineos ABS Lustran® 2783, Extrusion Grade
(discontinued **) Extrusion grade with super high impact.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a J.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
LyondellBasell Petrothene® NA960000 Low Density Polyethylene ApplicationsPETROTHENE NA960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA960 exhibits good unif.. |
|||
Vicat Softening Point | 92.0 °C @Load 5.00 kg |
198 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
Vicat Softening Point | 92.0 °C @Load 5.00 kg |
198 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical LI933 Co-Extrusion ASA Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical |
|||
Vicat Softening Point | >= 92.0 °C | >= 198 °F | ASTM D1525 |
Iran Petrochemical (PCC) HIPS 8350 High Impact Polystyrene HIPS 8350 is a very high impact polystyrene used in the extrusion industry. This grade has an improved environmental stress crack resistance (ESCR) in comparison with standard high impact polystyre.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525-95 |
Multibase Multi-ABS 801 Natural Extrusion Grade Data provided by Multibase. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® SF-0950S MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® TF-0959 T HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Noryl HIPS3191 PS This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
A. Schulman CP775-01 Molding Grade, Low Density Polyethylene DescriptionCp 755-01 is a molding grade, low-density polyethylene. ApplicationCP 755-01 meets the specification contained in FDA Regulation 177.1520 for food contact applications.Information provid.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | |
A. Schulman CP851 High Flow, Injection Molding Grade DescriptionCP 851 is a high flow injection molding grade of conventional (high pressure) low density polyethylene. ApplicationCP 851 meets the specifications in FDA Regulation 21 CFR177.1520 (c)3.1.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | |
A. Schulman CP851 High Flow, Injection Molding Grade DescriptionCP 851 is a high flow injection molding grade of conventional (high pressure) low density polyethylene. ApplicationCP 851 meets the specifications in FDA Regulation 21 CFR177.1520 (c)3.1.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Propionate 380A2R30015 Natural, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Propionate 384A4000016 Clear, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Dow 621I Low Density Polyethylene (LDPE) Specialty resin designed for high melt strength applications Provides excellent bubble stability Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Vicat Softening Point | 92.2 °C | 198 °F | |
Dow SE SLR-6410 Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-6410 is manufactured by anionic solution polymerization using lithium initiator and is extended with 50 parts of aromatic oil in relation to solid rubber. It is a product with medium styrene.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | DIN 53460 |
Ineos Nova S-4122 Medium Impact Compact Polystyrene
(discontinued **) Low friction, medium impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection moldin.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |