Polymer Property : Secant Modulus = 0.193 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.193 GPa
28.0 ksi
ASTM D638
NOVA Chemicals Novapol® LF-0222-A LDPE Wire and Cable Resin  (discontinued **)
NOVA Chemicals NOVAPOL® LF-0222-A is a medium molecular weight low density polyethylene. Resin consistency and purity are very high which make it suitable as a base resin in Wire and Cable applicat..
Secant Modulus 0.193 GPa
28.0 ksi
MD; ASTM D882
Teknor Apex Terraloy™ BP 10000A Thermoplastic Starch + LLDPE
Notes: Terraloy™ BP-10001A is a Thermoplastic Starch/LLDPE ready-to-process compound that contains up to 30% of TPS renewable content. This compound is for blown film application. Forms: Pellets A..
Secant Modulus 0.193 - 1.20 GPa
28.0 - 174 ksi
Average value: 0.545 GPa Grade Count:3
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..