Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® FL 20 Low Density Polyethylene - Blown Film Extrusion Riblene FL 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FL 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® FL 30 Low Density Polyethylene - Blown Film Extrusion Riblene FL 30 is a low density polyethylene (LDPE) ideal for blown film extrusion. Riblene FL 30 is characterized by a good balance between processability, mechanical and optical properties.Films m.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 250 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10 min |
Polimeri Europa KOBLEND HI PD 14 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend, similar to KOBLEND HI 18 with higher shrinkage values. Main application fields: bumpersUnfilled. Suitable for Injection .. |
|||
Melt Flow | 2.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM Data |
Americas Styrenics Styron® 685 Polystyrene
(discontinued **) STYRON® 685 general purpose polystyrene resin is a high heat resin used in consumer electronics and housewares. It offers excellent clarity, good moldability for use in hot runner systems. When use.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 4610 LDPE High Clarity, Bakery Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Clarity, Very High Gloss, Medium Slip, No Antiblock, Good Stability at High Drawdown Speeds, Good Printability, Good Heat Seal CharacteristicsApplic.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL NC010 is a high viscosity acetal homopolymer with 1.5% Teflon® PTFE Micropowder.Information provided by DuPont Performance Polymers |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LF-0222-A LDPE Wire and Cable Resin
(discontinued **) NOVA Chemicals NOVAPOL® LF-0222-A is a medium molecular weight low density polyethylene. Resin consistency and purity are very high which make it suitable as a base resin in Wire and Cable applicat.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LF-0225-B LDPE Clarity Film Resin
(discontinued **) Features: High optical clarityExcellent processability Applications: Produce and bakery filmLinersTextile packaging filmGeneral packaging requiring high clarity filmInformation provided by Nova Chem.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-129 MDPE Cast Overwrap Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-129 can be used in overwrap applications and in push-through .. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA951000 Low Density Polyethylene ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ASTM D1238 |
LyondellBasell Plexar® PX3060 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and .. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ASTM D1238 |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos J50-200-178 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the molding of screw caps dedicated to the packaging of carbonated beverages. This material m.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) LL0220AA Linear Low Density Polyethylene LL 0220 AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. This grade is suitable for the production of blown film for light duty applications and for the production of ca.. |
|||
Melt Flow | 2.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SD-0150W ABS, Unreinforced WNP GradeInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 800 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Borealis LR4201L Polyethylene Insulation Compound, Crosslinkable LR4201L is a natural low-density crosslinkable polyethylene compound. Application: LR4201L is designed as insulation compound for low voltage power cables. Specifications: IEC 60502 ANSI/ICEA S-66.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EF606 Low Density Polyethylene Westlake EF606 is a LDPE resin suggested for use in multiwall and general purpose liners, and for use as a blend resin in general purpose packaging applications. It has excellent processability, and.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips MarFlex® 5440 Low Density Polyethylene, Cast Film This LDPE is tailored for cast film applications that require:Suited for high speed convertingGood clarityLow coefficient of frictionTypical cast film applications include:Coextruded filmGeneral pur.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | Exxon Method |
ExxonMobil EXACT™ 4053 Plastomer for Film Applications Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ExxonMobil Method |
ExxonMobil EXACT™ 4151 Plastomer for Cast Film Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer multilayer coextru.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100TL NC010 (formerly Delrin 100TL NC000) is a high viscosity acetal homopolymer with 1.5% TeflonInformatio.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene TS9022 is a low-density polyethylene (LDPE) developed specially for automatic overwrap packaging. This resin has a combination of high optical properties and excellent stiffness. The incorporated ad.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ASTM D1238 |
Aclo Accucomp ABS ABS803L Medium Impact Grade |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | Condition G |
Ineos Nova 5490 High Impact Polystyrene
(discontinued **) High heat, Good environmental stress crack resistance, Excellent printabilityApplications: Custom sheet, Lithographic applicationsProperties were determined on injection molded specimens at 23°C an.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Exceed™ 2227ED Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2227ED is a metallocene ethylene-hexene copolymer. It offers an excellent balance of high modulus and impact strength. The higher melt index makes it ideally suited for L.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
BP Amoco Acclear® 6219 Homopolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Sheet extrusion; ThermoformingFeatures: High clarity, High heat resistance, Good melt strength/flow balanceTypical applications: Rigid packagingComplies with FDA speci.. |