Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 92.0 °C @Load 1.00 kg |
198 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Flexirene® MT 40 A Linear Low Density Polyethylene Flexirene MT 40 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Flexirene MT 40 A is characterized by a good processability and impact r.. |
|||
Vicat Softening Point | 92.0 °C @Load 1.00 kg |
198 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® MP 30 R Low Density Polyethylene - Injection Molding Riblene MP 30 R is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MP 30 R are characterized by a medium rigidity.Main Applications: Riblene MP 30 R is suitable for in.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Network Polymers MS 175 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY2010 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY6012 PC+ABS (Asia Pacific) Cycoloy* resin grade CY6012 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 & 5VB rating.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Huntsman PE1023 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good draw down characteristics.Applications: Film extrusion: drum liners, hardware packaging, and refuse bags.FDA Notes: Conforms to FDA regulation 21 CFR 17.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
LyondellBasell Petrothene® NA217000 Low Density Polyethylene ApplicationsPETROTHENE NA 217-000 is a high speed, lightweight coating resin for use with paper, films and other base stocks. This resin can yield coating weights down to 3.5 lbs/ream at line speed.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
LG Chemical SEETEC BF415 LDPE Characteristics: Good Processability and Excellent Optical Properties Applications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Hannam Chemical Hanalac 795 ABS, Pipe Grade Designed for pipe and bobbin sleeves. Excellent processability and high impact strength. Manufactured to prevent static electricity. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
LyondellBasell Petrothene® NA860008 Low Density Polyethylene ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5071 800 Micron LLDPE Powder Description: ICOFLO 510-5071 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Spartech Royalite R21M General Purpose ABS Resin Data provided by the manufacturer. A general-purpose ABS resin with high impact strength, R-21M is a popular choice for a variety of products, from bicycle helmets and carrying cases to portable ta.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® TF-0959 T HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
A. Schulman CP775-01 Molding Grade, Low Density Polyethylene DescriptionCp 755-01 is a molding grade, low-density polyethylene. ApplicationCP 755-01 meets the specification contained in FDA Regulation 177.1520 for food contact applications.Information provid.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | |
A. Schulman CP851 High Flow, Injection Molding Grade DescriptionCP 851 is a high flow injection molding grade of conventional (high pressure) low density polyethylene. ApplicationCP 851 meets the specifications in FDA Regulation 21 CFR177.1520 (c)3.1.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | |
A. Schulman CP851 High Flow, Injection Molding Grade DescriptionCP 851 is a high flow injection molding grade of conventional (high pressure) low density polyethylene. ApplicationCP 851 meets the specifications in FDA Regulation 21 CFR177.1520 (c)3.1.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Propionate 380A2R30015 Natural, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Chevron Phillips MarFlex® 1017 General Purpose Coating Resin Characteristics: Excellent Processability, High Temperature Stability, Low Neck-inApplications:Flexible Packaging, Laminations, Sealant Resin, General Purpose Coating ResinData provided by Chevron C.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | |
BASF Novolen® 1101 P Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | |
BASF Novolen® 1102 H Polypropylene Grade with high processing stability for packaging tapes, film tape, fibrillated film, monofilaments, thermoformed and blow molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Huntsman PE2035 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Medium flow resin with good stiffness.Applications: Injection molding: color concentrates.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under c.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Ineos Nova 3590 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable for difficult to fill and thin wall molding, Low residuals, USP Class VIApplications: Blending applications, Single service drinkware, Medical moldingExposure to g.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | DIN 53460 |
Ineos Nova S-4122 Medium Impact Compact Polystyrene
(discontinued **) Low friction, medium impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection moldin.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | |
BASF Novolen® 1104 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Huntsman PE8020 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total Lacqrene® 851 High Impact Polystyrene
(discontinued **) LACQRENE® 851 is a flame retardant, high impact polystyrene, halogen free rated UL 94 V0 @ 2.5 mm and UL 94 5VA @ 2mm. LACQRENE® 851 offers rheological and mechanics properties which permits larg.. |