NOVA Chemicals Novapol® HE-Y449-AC HDPE Extrusion Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HE-Y449-AC HDPE Extrusion Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium molecular weight HDPE, Good toughness, Good chemical resistance, Good processabilityApplications: Corrugated tubing, ConduitAdditives: AntioxidantsInformation provided by NOVA Chemicals.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D792
ESCR 100% Igepal® >= 1000 hour

@Temperature 50.0 °C
>= 1000 hour

@Temperature 122 °F
F<sub>50</sub>; Condition B; ASTM D1693
Oxidative Induction Time (OIT) 10 min
10 min
Condition 220°C in oxygen gas environment; ASTM D3895
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
Tensile Strength, Yield 24.0 MPa
3480 psi
Extension rate 2 in/min; ASTM D638
Elongation at Break 650 %
650 %
Extension rate 2 in/min; ASTM D638
Flexural Modulus 1.14 GPa
165 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 130 °C
266 °F
ASTM D3417
Vicat Softening Point 124 °C
255 °F
ASTM D1525
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D746