Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
ExxonMobil LL 8450 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50, condition B; ASTM D1693 |
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin
(discontinued **) Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.Applications: Extrusion on to metal pipes to produce a corrosion res.. |
|||
ESCR 100% Igepal® | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
Bent Strip, Condition A & B, F50 values, From compression molded samples; ASTM D 1693 |
NOVA Chemicals Novapol® TR-0535-UIG Hexene MDPE Rotational Molding Resin TR-0530-UIG complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UIG is .. |
|||
ESCR 100% Igepal® | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
Bent Strip, Condition B, F50 Values from compression molded samples; ASTM D 1693 |
NOVA Chemicals Surpass® RMs341-UG Octene sHDPE Rotational Molding Resin RMs341-UG complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A; ASTM D1693 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from .. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A; ASTM D1693 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from .. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A; ASTM D1693 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from .. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A; ASTM D1693 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from .. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A, F50; ASTM D-1693 |
Chevron Phillips Marlex® C100 Polyethylene; Enhanced Metallocene linear low density polyethylene. This linear low density, hexene copolymer is tailored for blow molded containers that require: High glossGood clarityExcellent ESCR Applications: Typi.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition B, F50; ASTM D-1693 |
Chevron Phillips Marlex® C300 Polyethylene; Enhanced Metallocene medium density polyethylene. This metallocene MDPE resin is tailored for blow molded containers that require: High glossGood clarityExcellent ESCR Applications: Typical blow molded ap.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A, F50; ASTM D-1693 |
Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced Low density linear polyethylene. This low density, linear resin is tailored for blow molded containers that require: Excellent processabilityExcellent ESCRApplications: Typical blow molded applica.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A, F50; ASTM D-1693 |
Chevron Phillips Marlex® HMN TR-935/935G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationExcellent impac.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A, F50; ASTM D-1693 |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
ExxonMobil LL 8450.31 Rotational Molding Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LLP 8450.31 Linear Low Density Polyethylene Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LLP 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
ESCR 100% Igepal® | >= 1000 hour @Thickness 2.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem GM7746C HDPE Blow Molding Polyethylene GM7746C is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tenac.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
ExxonMobil LL 8360 Rotational Molding Resin
(discontinued **) LL 8360 is a linear low density hexene copolymer designed to provide good processability along with outstanding dimensional control and low warpage. This resin is ideally suited for applications tha.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 Condition B |
ExxonMobil Paxon™ BA46-055 Blow Molding Resin Product Description: BA46-055 is a high molecular weight high density polyethylene copolymer. It possesses a combination of excellent processability, outstanding melt strength, high impact strength.. |