Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.14 GPa | 165 ksi | Tangent; ASTM D790 |
NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin Features: High ESCR, good toughness, good chemical resistance, good processability.Applications: Pipe coatings, profile extrusions, sheet extrusion for thermoforming, corrugated tubing, conduit.Data.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | Tangent; ASTM D790 |
NOVA Chemicals Novapol® HE-Y449-AC HDPE Extrusion Resin Medium molecular weight HDPE, Good toughness, Good chemical resistance, Good processabilityApplications: Corrugated tubing, ConduitAdditives: AntioxidantsInformation provided by NOVA Chemicals. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Petromont 4102 High Density Polyethylene Resin Petromont HDPE 4102 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is intended for general use in large diameter light weight drainage tubing applicat.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CR120CL Polypropylene, Random Copolymer, Clarified, Lubricated Random clarified copolymer specially formulated to achieve high clarity and excellent color and color stability with excellent mold release properties. Applications: Injection molding applications s.. |
|||
Flexural Modulus | 1.14 - 5.10 GPa | 165 - 740 ksi | Average value: 2.06 GPa Grade Count:118 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | at 0.05 in/min; ASTM D790 |
M. Holland Company CP400 Polypropylene Copolymer Features: Medium Flow, High Impact ResistanceUses: Appliances, Business Equipment, Construction Applications, Tool/Tote Box, ToysProcessing Method: Injection MoldingInformation provided by M. Hollan.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
LyondellBasell Petrothene® LP5100 High Density Polyethylene ApplicationsPETROTHENE LP 5100 is especially designed for large-part blow molding of durable goods and deep-draw sheet extrusion/thermoforming applications. LP 5100 exhibits excellent impact resist.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Kostat ICP-STAT ICD-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790A |
Ineos N00G-01 Polypropylene Impact Copolymer Grade N00G-01 is a fractional melt flow rate impact copolymer for blow molding, pipe, tubing, and sheet extrusion. It offers a good balance of stiffness and impact strength as compared to other impa.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Spartech Marballoy Marbleized Thermoplastic Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Spartech Soft Touch HDPE Polyolefin Skin/Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Spartech SP-1510 Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Spartech Ultros SRP Co-Extruded Skid-Resistant PE Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY 63000CT PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Techmer ES Statiblend® 02036 Polypropylene Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 3312E Random Copolymer Polypropylene Random Copolymer for Storage Boxes, Pill Vials and Containers Formolene® 3312E is a clarified, medium flow random copolymer with fast cycle time and easy mold release. It is designed for injection .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | |
CMW® ELKONITE® 40W3 Infiltrated Tungsten Copper material ASTM B702 For vacuum switch contacts, low expansion structural members.Information provided by CMW Inc. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Rilsan® PA 11 G BMNO MED Nylon 11 Rilsan® PA 11 G BMNO MED is a polyamide produced from a renewable source. This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applic.. |
|||
Flexural Modulus | 1.14 - 6.21 GPa | 165 - 900 ksi | Average value: 3.16 GPa Grade Count:42 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |