Multibase Nylex™ 4650 Polyamide + PP

Category Polymer , Thermoplastic , Nylon , Polypropylene (PP)
Manufacturer Multibase
Trade Name Nylex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Nylex™ 4650 Polyamide + PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mineral filler, 33% Filler by WeightForms: PelletsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM 792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 68.9 MPa
10000 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 5.17 GPa
750 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
73°F; ASTM D256
Gardner Impact 1.017 J
0.7500 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 186 °C
367 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 161 °C
322 °F
Unannealed; ASTM D648
Vicat Softening Point 198 °C
388 °F
ASTM D1525
Flammability, UL94 HB
HB