Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
PolyOne Maxxam™ MN-818.S001-8000 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | <= 114 MPa | <= 16500 psi | ISO 178 |
Polykemi AB SCANMID 6 B12^ NH11L Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N2300HL BK Post Consumer Recycle Nylon 6 Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N2300HL BK/UV2 Post Consumer Recycle Nylon 6 Heat Stabilized, Lubricated, UV Stabilized, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
PolyOne Edgetek® AS-20GF/000 HI UV NAT Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **)& Description/Features:Glass Fiber ReinforcedHigh ImpactUV StabilizedNaturalUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000L2 Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Techmer ES Electrablend® PC 04008 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Techmer ES Electrablend® PC 04009 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal LNP STAT-KON* KEP33 is a compound based on Acetal resin containing 15% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Chase Plastics CP Pryme® N100M2 (Dry) Nylon 6, Lubricated Features: DurableLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Chase Plastics CP Pryme® N100MD2 (DAM) Nylon 6 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Flexural Strength | 114 MPa | 16500 psi | Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Adell AS-30 Nylon 66, General Purpose Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-40FM-B269 40% Glass/Mineral Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 631 Nylon 6/6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
PolyOne Edgetek® AT-20GF/000 FDA Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 114 MPa @Temperature 175 °C |
16500 psi @Temperature 347 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |