ChevronTexaco Regal® AW 100

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Regal® AW 100.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Regal AW oil delivers value through:High Temperature stability provides long lubricant life and resistance to formation of sludge and varnish on bearings and gears.Excellent wear protection provides long bearing life and protects gears from scuffing.Excellent water separability provides benefits for circulating oil systems subject to severe water contaminationEffective foam inhibition — Reduces the amount of entrained air in the oil, minimizing the possibility of pump cavitation and also prevents surface foam.Texaco Regal AW 100 is a circulating oil formulated from high quality base stocks and a carefully balanced, zinc-free additive package. This provides excellent protection against wear for long bearing and gear life. Texaco Regal AW 100 has superior water separability properties and rust protection to deal with the severe water contamination that frequently occurs in circulating oil systems. Its outstanding oxidation stability minimizes deposit formation and leads to long lubricant life. Texaco Regal AW 100 is a circulating oil designed for the steel industry. It is formulated to meet the needs of circulation systems serving high speed rollers and plain bearings in no-twist finishing mills It is also recommended for the lubrication of reduction gears and bearings where zinc-free oils are desired. Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 220628; MSDS Number: 8782
Physical Properties Metric English Comments
API Gravity 31.2 °
31.2 °
Viscosity Measurement 105
105
Viscosity Index
Saybolt Viscosity at 100°F 494 SUS
494 SUS
Saybolt Viscosity at 210°F 65 SUS
65 SUS
Kinematic Viscosity at 40°C (104°F) 95 cSt
95 cSt
Kinematic Viscosity at 100°C (212°F) 11.3 cSt
11.3 cSt
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
Flash Point 276 °C
529 °F
Descriptive Properties Value Comments
FZG Pass Stage 13
DIN 51354
Rust Prevention Pass
SSW