Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
NYCOA 534 H High Viscosity, Heat Stabilized Nylon 6 Resin NYCOA 534 H is a high viscosity; heat stabilized, nucleated Nylon 6 resin. The high viscosity and fast set-up time make an excellent material for extrusion of tubing, rods, sheet and film. Because o.. |
|||
Flexural Strength | <= 114 MPa | <= 16500 psi | ISO 178 |
Polykemi AB SCANMID 6 B12^ NH11L Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N2300HL BK Post Consumer Recycle Nylon 6 Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N2300HL BK/UV2 Post Consumer Recycle Nylon 6 Heat Stabilized, Lubricated, UV Stabilized, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6 Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32 PC LNP LUBRICOMP* DFL32 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Resinoid 1382 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
PolyOne Edgetek® AS-20GF/000 HI UV NAT Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **)& Description/Features:Glass Fiber ReinforcedHigh ImpactUV StabilizedNaturalUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Techmer ES Electrablend® PC 04008 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Techmer ES HiFill FR® ABS GF30 FR 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 114 MPa | 16500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX04522C PC (Asia Pacific) LNP Stat-Kon DX04522C is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: High Modulus, Electrically Conductive, Clean Compound System. Also .. |
|||
Flexural Strength | 114 MPa | 16500 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX11411 PC LNP* STAT-KON* DX11411 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal LNP STAT-KON* KEP33 is a compound based on Acetal resin containing 15% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Techmer ES Plaslube® J-50/10/TF/15 BK223 Polycarbonate |
|||
Flexural Strength | 114 MPa | 16500 psi | at rupture; ASTM D790 |
Sumitomo Bakelite North America E 8701A Short Glass Fiber Reinforced Epoxy E 8701A is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North Amer.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Chase Plastics CP Pryme® N100MD2 (DAM) Nylon 6 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 651 Nylon 6, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.35% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Adell AS-30 Nylon 66, General Purpose Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-40FM-B269 40% Glass/Mineral Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 262 Glass Reinforced, Modified SMA Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
PolyOne Edgetek® AT-20GF/000 FDA Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation. |