Ashley Polymers Ashlene® R6043 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® R6043 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium viscosity extrusion grade Nylon 6 resin with excellent melt stability, good melt strength: suitable for extrusion coating and film co-extrusion applications. Excellent grease resistance, toughness, resistance to abrasion; doesn't absorb food odorsData provided by the manufacturer
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 82.8 MPa
12000 psi
ATSM D638
Tensile Strength, Yield 82.8 MPa
12000 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Strength 103 MPa
14900 psi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D3418
Processing Properties Metric English Comments
Processing Temperature 249 - 260 °C
480 - 500 °F
at die