Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Omni Plastics OmniTuff™ HPP GRC10 MI30 Homopolymer Polypropylene Glass/Mineral Filled Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
PolyOne Edgetek® PK-10GF/000 Polyetheretherketone (PEEK) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6 (Asia Pacific) LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Techmer ES HiFill FR® ABS GF20 FR RD073 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Flame RetardantAppearance: RedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Techmer ES HiFill® PP 0202 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/ABS 1120 GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInformation p.. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Techmer ES HiFill® PP GF/M35 CC BK 35% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RX93402 PA 66 LNP THERMOCOMP* RX93402 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
PlastxWorld CEVIAN® A2604 20% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM Test |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR15 Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
PolyOne Edgetek® PF-10GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |