Material Notes:
Key Features: medium melt flow, very high modulus, UV-stabilized thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent weatherability, high stiffness, good dimensional stabilityApplications: molded-in color automotive claddings and rocker panels, license plate brackets, appliquesDescription: Hifax BB222GC medium melt flow, UV-stabilized, weatherable, mineral-filled thermoplastic elastomeric olefin resin has an excellent balance of rigidity, low temperature impact and dimensional stability. It was designed for a variety of molded-in color automotive exterior ornamentation applications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
Tool, Montell
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ISO 868
Tensile Strength, Ultimate 14.0 MPa
2030 psi
ISO R527-1
Tensile Strength, Yield 21.0 MPa
3050 psi
ISO R527-1
Elongation at Break 100 %
100 %
ISO R527-1
Elongation at Yield 7.0 %
7.0 %
ISO R527-1
Flexural Modulus 2.00 GPa
290 ksi
ISO 178
Izod Impact, Notched 0.230 J/cm

@Temperature -40.0 °C
0.431 ft-lb/in

@Temperature -40.0 °F
ISO 180
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature -30.0 - 100 °C
27.8 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ISO 75