Lehmann & Voss LUVOCOM® 3-8277 Polyamide 6, unreinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 3-8277 Polyamide 6, unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduced moment of inertia compared with metal parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.011 - 0.016 cm/cm
0.011 - 0.016 in/in
Mechanical Properties Metric English Comments
Tensile Stress 65.0 MPa
9430 psi
Elongation at Yield 2.8 %
2.8 %
3.6 %
3.6 %
flexural
Modulus of Elasticity 3.50 GPa
508 ksi
Flexural Strength 90.0 MPa
13100 psi
Flexural Modulus 3.00 GPa
435 ksi
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
edgewise; ISO 179 1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
120 °C
248 °F
short term
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+10 ohm
>= 1.00e+10 ohm
Insulation Resistance >= 1.00e+10 ohm
>= 1.00e+10 ohm
Processing Properties Metric English Comments
Processing Temperature 270 °C
518 °F
mass temp
Nozzle Temperature 270 - 280 °C
518 - 536 °F
Zone 1 250 - 270 °C
482 - 518 °F
Zone 2 270 - 290 °C
518 - 554 °F
Zone 3 280 - 300 °C
536 - 572 °F
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Drying Temperature 75.0 °C

@Time 36000 - 57600 sec
167 °F

@Time 10.0 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
or
Descriptive Properties Value Comments
Color black blue