Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.50 GPa | 508 ksi | 50% RH |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ASTM D638 |
Ineos Nova 3930 General Purpose Crystal Polystyrene
(discontinued **) High melt flow, Crystal clearApplications: Razor components, Personal care, Thin wall moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and .. |
|||
Modulus of Elasticity | 3.50 - 12.2 GPa | 508 - 1770 ksi | Average value: 5.54 GPa Grade Count:33 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Modulus of Elasticity | 3.50 - 19.0 GPa | 508 - 2760 ksi | Average value: 9.24 GPa Grade Count:75 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1105-7301 PEEK, unreinforced, laser markable Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1106-8089/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 19-8073 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 19-8074 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 3-8277 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | Sample Type 1B, 50 mm/min; ISO 527-1/2:1993 |
Global EPP PA 6E Extruded Polyamide 6 Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 527-2 |
Tisan TISLAMID® 66 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 15MB440 OPP Film Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin .. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 25MB400 OPP Film Product Description: Heat seal coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 25MB400 can be either used as mono material or in laminated st.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 32MB768 OPP Film Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 40MB666 OPP Film Product Description: A is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle Ea.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 30LL666 OPP Film Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LL210 OPP Film Product Description: An uncoated biaxially oriented, transparent polypropylene film for Pressure Sensitive labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LL539 OPP Film Product Description: A clear, two-side coated, polypropylene label face stock designed for demanding pressure sensitive applications where outstanding ink adhesion and adhesive anchorage are require.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 30MM680 OPP Film Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS .. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 57LL210 OPP Film Product Description: An uncoated biaxially oriented, transparent polypropylene film for Pressure Sensitive labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 V15 Nylon 66, 15% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Modulus of Elasticity | 3.50 GPa @Temperature 60.0 °C |
508 ksi @Temperature 140 °F |
ISO 527 |
BASF Ultramid® KR 4350 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 178 |
Addiplast Addinyl A2 1 Flame Retardant Nylon 66 Flame retardant, halogen freeInformation provided by Addiplast. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 ZV15 Nylon 66, 15% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 527-1/-2 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 527-1/-2 |
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 527 |
BASF Ultramid® C3U PA66/6 (Dry) Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 527-2 |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |