Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.50 GPa | 508 ksi | 50% RH |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |
|||
Modulus of Elasticity | 3.50 - 12.2 GPa | 508 - 1770 ksi | Average value: 5.54 GPa Grade Count:33 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1106-8085/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 19-7969 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 19-8073 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 19-8074 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 3-8277 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 6-8512 Polyamide 12, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Especially suitable at dynamic.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | Sample Type 1B, 50 mm/min; ISO 527-1/2:1993 |
Global EPP PA 6E Extruded Polyamide 6 Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 15MB440 OPP Film Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin .. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 25MB866 OPP Film Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side PVOH. It provides excellent gas and aroma protection and is designed to be use.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 30MB400 OPP Film Product Description: A heat sealable coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 30MB400 can be either used as mono material or in lamina.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 30MBR666 OPP Film Product Description: Bicor 30MBR is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high moist.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 32MB768 OPP Film Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 40MB668 OPP Film Product Description: A high speed transparent biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides excellent perfo.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 17LL222 OPP Film Product Description: An uncoated biaxially oriented, transparent polypropylene film designed for overlamination in labeling applications where high gloss and high transparency are required.Availabil.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 30LL666 OPP Film Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 35LL400 OPP Film Product Description: A one-side treated, transparent coextruded OPP film. The film is slip controlled for optimal performance on reel-fed labeling machines.Availability: Africa & Middle East, Asia .. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LGT702 OPP Film Product Description: A transparent biaxially oriented polypropylene film coated one side resistant coating and one side with a specially formulated acrylic coating. This film is designed for cut and.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LL539 OPP Film Product Description: A clear, two-side coated, polypropylene label face stock designed for demanding pressure sensitive applications where outstanding ink adhesion and adhesive anchorage are require.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 30MM680 OPP Film Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS .. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 57LL210 OPP Film Product Description: An uncoated biaxially oriented, transparent polypropylene film for Pressure Sensitive labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 V15 Nylon 66, 15% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 ZV15 Nylon 66, 15% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | Conditioned; ISO 178 |
Addiplast Addinyl B2 G10 V20 Nylon 6, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 527-1/-2 |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 527-1/-2 |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 527-1/-2 |
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Modulus of Elasticity | 3.50 GPa | 508 ksi | ISO 527 |
BASF Ultramid® C3U PA66/6 (Dry) Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance. |