Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Carbon Fiber Reinforced
Manufacturer Lehmann & Voss & Co.
Trade Name ELECTRAFIL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss ELECTRAFIL M-2386 Polycarbonate, with carbon fiber and PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved friction and wear behaviour. Emergency running property.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance range.Body and duty parts in office equipment, gear wheels, grippers.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ISO 1183
Water Absorption <= 0.20 %
<= 0.20 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Stress 100 MPa
14500 psi
Elongation at Yield 2.5 %
2.5 %
3.0 %
3.0 %
flexural
Modulus of Elasticity 7.00 GPa
1020 ksi
Flexural Strength 140 MPa
20300 psi
Flexural Modulus 6.00 GPa
870 ksi
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
flatwise; ISO 179 1fU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179 1eA
Coefficient of Friction, Dynamic 0.25
0.25
Coefficient of Friction, Static 0.20
0.20
Thermal Properties Metric English Comments
CTE, linear 28.0 µm/m-°C
15.6 µin/in-°F
DIN 53752
Maximum Service Temperature, Air 130 °C
266 °F
150 °C
302 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
Vicat Softening Point 160 °C
320 °F
DIN ISO 306
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
Insulation Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
Processing Properties Metric English Comments
Processing Temperature 295 °C
563 °F
mass temp
Nozzle Temperature 290 - 310 °C
554 - 590 °F
Zone 1 280 - 300 °C
536 - 572 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 300 - 320 °C
572 - 608 °F
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Drying Temperature 120 °C

@Time 14400 - 21600 sec
248 °F

@Time 4.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color black
Users viewing this material also viewed the following: