LG Chemical 402 AF Flame Retardant HIPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical 402 AF Flame Retardant HIPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include televisions, VTR, monitors, computers and other electrical electronic parts requiring flame retard
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength, Yield 27.5 MPa
3990 psi
50 mm/min; ASTM D638
Elongation at Break 60 %
60 %
50 mm/min; ASTM D638
Flexural Yield Strength 46.2 MPa
6700 psi
15 mm/min; ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
15 mm/min; ASTM D790
Izod Impact, Notched 0.740 J/cm

@Thickness 6.35 mm
1.39 ft-lb/in

@Thickness 0.250 in
ASTM D256
1.03 J/cm

@Thickness 3.17 mm
1.93 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C

@Thickness 12.7 mm
169 °F

@Thickness 0.500 in
Unannealed; ASTM D648
Vicat Softening Point 94.0 °C
201 °F
1000 g; ASTM D1525
Flammability, UL94 V-2
V-2
1/8 in
V-2
V-2
1/16 in
Electrical Properties Metric English Comments
Arc Resistance 120 - 180 sec
120 - 180 sec
UL Rating PLC 5 (120-180 sec)
Comparative Tracking Index 400 - 600 V
400 - 600 V
UL Rating PLC 1 (400-600 volts)
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL Rating PLC 3 (15-30 sec)
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
UL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL Rating PLC 1 (10-25.4 mm/min)
Descriptive Properties Value Comments
IEC 707 Flammability FV2 mm/min.
1/16 in