Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.03 J/cm @Temperature -40.0 °C |
1.93 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 383A4000011 Cellulose Acetate Propionate, Clear, Trsp Applications:AppliancesFloor carePersonal care and cosmeticsProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, stren.. |
|||
Izod Impact, Notched | 1.03 J/cm @Thickness 3.17 mm |
1.93 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical 402 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include t.. |