Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Asia Pacific) PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1... |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® EHA PC+ABS PC+ABS. Electroplateable. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | PLC code 3; UL 746A |
SABIC Innovative Plastics Cycoloy® FXC810FE PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810FE is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ferrite colour effects. The colour package may effect performance.This data was supp.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | PLC code 3; UL 746A |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® LUX2114G PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® LUX9610 PC (Asia Pacific) Lexan LUX9610 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS require.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Europe-Africa-Middle East) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific) ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® LUX9612 PC (Asia Pacific) Lexan LUX9612 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
LG Chemical 20HRI GPPS Heat resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, S.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=0.750 mm |
15 - 30 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=0.750 mm |
15 - 30 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2330A(W) PA6+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Cooling Fan), E&E (Bobbin)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=0.750 mm |
15 - 30 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
LG Chemical MI-730 MIPS |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
LG Chemical MI-750 MIPS Medium impact |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
LG Chemical 92HR SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | |
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | PLC code 3; UL 746A |
SABIC Innovative Plastics Prevex VFAX PPE+PS High impact strength. 180F (82C) HDT. Improved productivity/reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Valox® DR48 PBT 17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Valox® 451E PBT 20% GR. Easy flow version of VALOX 451. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C6303 PC+ABS LNP* Lubricomp* Cycoloy_C6303 compound is a Wear resistant (5% PTFE), flame retardant PC+ABS. High heat and good hydrolytic stability. UL listing from Japan and Pacific. |