Polymer Property : Flexural Yield Strength = 6700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 46.2 - 108 MPa
6700 - 15700 psi
Average value: 88.8 MPa Grade Count:13
Overview of materials for Chlorinated PVC (CPVC)
This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr..
Flexural Yield Strength 46.2 MPa
6700 psi
15 mm/min; ASTM D790
LG Chemical 501S-S HIPS
Self lubricant, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food holders, par..
Flexural Yield Strength 46.2 MPa
6700 psi
15 mm/min; ASTM D790
LG Chemical 60HR HIPS
Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape recorders, vacu..
Flexural Yield Strength 46.2 MPa
6700 psi
ASTM D790
Techmer ES HiFill® PP GF30 TL15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: LubricatedInformation provided by TP Composites..
Flexural Yield Strength 46.2 MPa
6700 psi
ASTM D790
PlastxWorld CEVIAN® A1700 PA/ABS Alloy, Conditioned
Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc.
Flexural Yield Strength 46.2 MPa
6700 psi
15 mm/min; ASTM D790
LG Chemical 402 AF Flame Retardant HIPS
NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include t..