Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Prevex VFAX PPE+PS High impact strength. 180F (82C) HDT. Improved productivity/reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem AUT230M PEI Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are .. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem AUT230M PEI (Europe-Africa-Middle East) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su.. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem XH6050F PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was .. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi.. |
|||
Izod Impact, Notched | 0.740 J/cm @Thickness 6.35 mm |
1.39 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
LG Chemical 402 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include t.. |