Material Notes:
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Linear Mold Shrinkage, Flow 0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
Linear Mold Shrinkage, Transverse 0.0125 - 0.0155 cm/cm
0.0125 - 0.0155 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
Elongation at Break 7.5 %
7.5 %
Elongation at Yield 3.0 %
3.0 %
Tensile Modulus 3.80 GPa
551 ksi
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
Charpy Impact, Notched 0.330 J/cm²
1.57 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Vicat Softening Point 230 °C

@Load 5.00 kg
446 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Volume Resistivity 200 ohm-cm
200 ohm-cm
Surface Resistance 20 ohm
20 ohm
Processing Properties Metric English Comments
Melt Temperature 230 - 250 °C
446 - 482 °F
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Drying Temperature 90.0 - 100 °C
194 - 212 °F
Descriptive Properties Value Comments
Electromagnetic reflection 96 dB
ISO Shrinkage - Pressure 60 MPa