Electrical Properties Metric English Comments
Volume Resistivity 200 ohm-cm
200 ohm-cm
53 parts per 100 of NC E128-02 in the final compound
Nanocyl EPOCYL™ NC E128-02 Master Batch Liquid Bisphenol-A Resin for non-Solvent Based Formulation Purposes
EPOCYL™ NC E128-02 is a Mater Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed to enh..
Volume Resistivity 200 ohm-cm
200 ohm-cm
LATI Latiohm 85-06 PD01 G/15 PES, 15% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyether Sulfone (PES). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Volume Resistivity 200 ohm-cm
200 ohm-cm
LATI Latishield 66-10A G/15 PA66, Steel/Glass Fiber Reinforced
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Volume Resistivity 200 ohm-cm
200 ohm-cm
LATI Latishield 66-10A H2 CETG/400 PA66, Steel/Glass Fiber Reinforced, Mineral Filled, Heat Stabilized
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Volume Resistivity 200 ohm-cm
200 ohm-cm
LATI Latishield 66-10A PA66, Steel Fiber Reinforced
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Volume Resistivity 200 ohm-cm

@Time 420 sec
200 ohm-cm

@Time 0.117 hour
18% Carbon Black
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
Volume Resistivity 200 ohm-cm
200 ohm-cm
IEC 60093
Polyplastics Duracon® CH-15 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance