Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00900 - 0.0155 cm/cm | 0.00900 - 0.0155 in/in | Average value: 0.0127 cm/cm Grade Count:12 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Linear Mold Shrinkage, Transverse | 0.0125 - 0.0155 cm/cm | 0.0125 - 0.0155 in/in | |
LATI Latamid 66 PA 66 Polyamide 66 (PA66). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Linear Mold Shrinkage, Transverse | 0.0125 - 0.0155 cm/cm | 0.0125 - 0.0155 in/in | |
LATI Latilub 66-02S PA66, Silicone Filled Self-lubricating product based on Polyamide 66 (PA66). Silicone. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.0155 cm/cm | 0.012 - 0.0155 in/in | |
LATI Latiohm 88/10-06 CNT PEEK Semiconductive/dissipative product based on Polyetheretherketone (PEEK). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Linear Mold Shrinkage, Transverse | 0.0125 - 0.0155 cm/cm | 0.0125 - 0.0155 in/in | |
LATI Latishield 66-10A PA66, Steel Fiber Reinforced EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Linear Mold Shrinkage, Transverse | 0.0125 - 0.0155 cm/cm | 0.0125 - 0.0155 in/in | |
LATI Latistat 66-06 PA66 Dissipative product based on Polyamide 66 (PA66). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Linear Mold Shrinkage, Transverse | 0.0125 - 0.0155 cm/cm | 0.0125 - 0.0155 in/in | |
LATI Latilub 66-01M PA66, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Linear Mold Shrinkage, Transverse | 0.0125 - 0.0155 cm/cm | 0.0125 - 0.0155 in/in | |
LATI Latimass 52/11-01 D020 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Transverse | 0.0125 - 0.0155 cm/cm | 0.0125 - 0.0155 in/in | |
LATI Latimass 53-04 D009 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |