LATI Laticonther 87/28 GR/50 PC, 50% Graphite Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer LATI
Trade Name Laticonther
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Laticonther 87/28 GR/50 PC, 50% Graphite Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High thermal conductivity product based on Polycarbonate (PC). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
Linear Mold Shrinkage, Flow 0.0045 - 0.0070 cm/cm
0.0045 - 0.0070 in/in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0075 cm/cm
0.0050 - 0.0075 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
Elongation at Break 0.80 %
0.80 %
Tensile Modulus 7.00 GPa
1020 ksi
Charpy Impact Unnotched 0.800 J/cm²
3.81 ft-lb/in²
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
Thermal Properties Metric English Comments
Thermal Conductivity 10.0 W/m-K
69.4 BTU-in/hr-ft²-°F
Longitudinal
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
Vicat Softening Point 145 °C

@Load 5.00 kg
293 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 8000 ohm
8000 ohm
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 100 - 120 °C
212 - 248 °F
Drying Temperature 120 - 130 °C

@Time 10800 sec
248 - 266 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa