Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0040 - 0.0075 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0075 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Geloy XTWM206 ASA
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.0040 - 0.0075 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0075 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Geloy XTWM206 ASA (Asia Pacific)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Asia Pacific regio..
Linear Mold Shrinkage, Transverse 0.0040 - 0.0075 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0075 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm
0.0055 - 0.0075 in/in
LATI Lastilac 10 ABS/PC
ABS/PC Blend (ABS/PC). Unfilled. Very good surface appearance. High impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI..
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm
0.0055 - 0.0075 in/in
LATI Latamid 6 H2E04 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. Glass fibers. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm
0.0055 - 0.0075 in/in
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0075 cm/cm
0.0050 - 0.0075 in/in
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm
0.0055 - 0.0075 in/in
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0075 cm/cm
0.0050 - 0.0075 in/in
LATI Laticonther 87/28 GR/50 PC, 50% Graphite Reinforced
High thermal conductivity product based on Polycarbonate (PC). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
LATI Latilon 28D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
LATI Latilon 30D G/10-V0 PC, 10% Glass Fiber Reinforced, Flame Retardant
Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
LATI Latilub 87/24UV-20T PC, PTFE Filled
Self-lubricating product based on Polycarbonate (PC). UV stabilized. PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
LATI Latilub 87/28-20T PC, PTFE Filled
Self-lubricating product based on Polycarbonate (PC). PTFE.Information provided by Lati Industria Termoplastici S.p.A.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0075 cm/cm
0.0050 - 0.0075 in/in
LATI Latiohm 87/26-06 PD01-V1 PC, Flame Retardant
Semiconductive/dissipative product based on Polycarbonate (PC). UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
LATI Latiohm 87/28-07 CNT PC
Semiconductive/dissipative product based on Polycarbonate (PC). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm
0.0055 - 0.0075 in/in
LATI Latishield 36/AR-08A G/17-V0E ABS, Steel/Glass Fiber Reinforced, Flame Retardant
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
LATI Latishield 87/28-10A PC, Steel Fiber Reinforced
EMI shielding product based on Polycarbonate (PC). Steel fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas..
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm

@Thickness 3.20 mm
0.0055 - 0.0075 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS
PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers.
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm

@Thickness 3.00 mm
0.0055 - 0.0075 in/in

@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Covestro Bayblend® M850 XF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas..
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm

@Thickness 3.00 mm
0.0055 - 0.0075 in/in

@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Covestro Bayblend® T50 BBS083 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Goo..
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm

@Thickness 3.00 mm
0.0055 - 0.0075 in/in

@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Covestro Bayblend® T80 XG PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Opt..
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm

@Thickness 3.00 mm
0.0055 - 0.0075 in/in

@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Covestro Bayblend® T85 SG PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Hig..
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm
0.0055 - 0.0075 in/in
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion ..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
LATI Latilon 30D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
LATI Latilub 80-15T G/30 PPS, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
LATI Latilub 80-17ST G/30 PPS, 30% Glass Fiber Reinforced, Silicone/PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid..
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
LATI Kelon® A FR H2 CET/35-V2 PA 66, 35% Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; La..