Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 8000 ohm | 8000 ohm | |
LATI Laticonther 87/28 GR/50 PC, 50% Graphite Reinforced High thermal conductivity product based on Polycarbonate (PC). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Surface Resistance | 8000 ohm | 8000 ohm | IEC 60093 |
Polyplastics Duracon® CH-10 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |