Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Mold Temperature = 100 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 100 - 120 °C
212 - 248 °F
NHEP Spectron™ E6666 Nylon 66, 30% Glass Fiber
Natural color. E6666 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati..
Mold Temperature 100 °C
212 °F
Optimum
Celanese Thermx® CG033 PCT, 30% Glass Reinforced  (Unverified Data**)
Thermx® CG033 is a 30% glass fiber reinforced polycyclohexylenedimethylene terephthalate for injection molding.30% glass, general purposeInformation provided by Celanese
Mold Temperature 100 °C
212 °F
Optimum
Celanese Thermx® CG923 PCT, 20% Glass Reinforced  (Unverified Data**)
Thermx® CG923 is a 20% glass fiber reinforced and flame retardant polycyclohexylenedimethylene terephthalate for injection molding.20% glass fiber reinforced, flame retardantInformation provided by..
Mold Temperature 100 - 150 °C
212 - 302 °F
LATI LAESTRA E01 G/30 30% Glass Fiber Reinforced, Elastomer Modified Syndiotactic Polystyrene (SPS)  (disconti
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..
Mold Temperature 100 °C
212 °F
Injection Molding
Covestro Apec® DP 1-9379/5 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba..
Mold Temperature 100 - 120 °C
212 - 248 °F
LATI LATILUB 95-25GR CE/10 Polysulfone Base (PSU), 25% Graphite, 10% Special Mineral Filled Self Lubricating Plastic
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Mold Temperature 100 °C
212 °F
Injection molding; ISO 294
Celanese VECTRA E820iPd LCP, 40% Specialty  (Unverified Data**)
Catalytically modified E820i40 % mineral , excellent flow, electrolytic metal platableA three-zone screw evenly divided into feed, compression, and metering zones is preferred. A higher percentage ..
Mold Temperature 100 °C
212 °F
DAM; optimum
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSLR NC010 is a 25% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Mold Temperature 100 °C
212 °F
DAM; optimum
DuPont Performance Polymers Zytel® 70G35EF NC010 Nylon 66  (Unverified Data**)
Zytel® 70G35EF NC010 is a 35% glass reinforced polyamide 66 developed for electrical and electronics applications.Information provided by DuPont Performance Polymers
Mold Temperature 100 °C
212 °F
DAM; optimum
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6  (Unverified Data**)
Minlon® 73GM40 NC010 is a 40% mineral/glass reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Mold Temperature 100 - 140 °C
212 - 284 °F
Injection Molding
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Mold Temperature 100 - 120 °C
212 - 248 °F
LATI Laticonther 87/28 GR/50 PC, 50% Graphite Reinforced
High thermal conductivity product based on Polycarbonate (PC). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Mold Temperature 100 °C
212 °F
Taiwan PU Corporation PPG CPU-2172 Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Mold Temperature 100 °C
212 °F
Taiwan PU Corporation PTMG CPU-100L Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Mold Temperature 100 °C
212 °F
Taiwan PU Corporation PTMG CPU-42L Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Mold Temperature 100 - 110 °C
212 - 230 °F
actual surface temp
Unitika TERRAMAC TE-7307 Polylactic Acid (PLA)
Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Mold Temperature 100 - 120 °C
212 - 248 °F
Covestro Apec® 1695 Polycarbonate
Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content
Mold Temperature 100 °C
212 °F
Injection Molding; ISO 10724
Covestro Apec® 2095 Polycarbonate
Easy flowingeasy to demoldsoftening temperature (VST/B 120)=203 °CPreprocessingMax. Water content
Mold Temperature 100 °C
212 °F
Injection Molding; ISO 10724
Covestro Apec® 2097 Polycarbonate
Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=202 °CPreprocessingMax. Water content
Mold Temperature 100 °C
212 °F
Injection molding; ISO 294
Covestro Apec® FR1892 High-Heat Polycarbonate
This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along..
Mold Temperature 100 - 110 °C
212 - 230 °F
BASF Petra® 7010 WT 7729 15% Glass Filled PET
Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface ..
Mold Temperature 100 °C
212 °F
Optimum
Celanese Thermx® CG033 BK010T PCT
Thermx® CG033 BK010T is a 30% glass fiber reinforced, black polycyclohexylenedimethylene terephthalate resin for injection molding.Celenese acquired the Thermx product line from DuPont in 2010.
Mold Temperature 100 °C
212 °F
Optimum
Celanese Thermx® CG933 BK010 PCT
Thermx® CG933 BK010 is a 30% glass reinforced, flame retardant, black polycyclohexylenedimethylene terephthalate resin for injection molding.Celenese acquired the Thermx product line from DuPont in..
Mold Temperature 100 °C
212 °F
ISO 294
Celanese VECTRA B230 LCP, 30% Specialty
Exceptional strength and stiffness. Suitable for metal replacement applications. Electrically conductive. 30% carbon fiber reinforced.Information provided by Celanese
Mold Temperature 100 °C
212 °F
ISO 294
Celanese VECTRA E130i LCP, 30% Glass Reinforced
High temperature capability, easiest flow. Suitable where very thin walls are required. Used for broad range of SMT applications, with minimal dimensional change. 30% glass filled.Information provid..
Mold Temperature 100 °C
212 °F
Optimal
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
Mold Temperature 100 °C
212 °F
optimum
DuPont Performance Polymers Sorona® 3301 BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&l
Sorona® 3301 BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature condi..
Mold Temperature 100 °C
212 °F
optimum
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&l
Sorona® 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature conditions...
Mold Temperature 100 °C
212 °F
optimum
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont..
Mold Temperature 100 - 150 °C
212 - 302 °F
LATI LAESTRA G/40 40% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)  (discontinued **)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..
Copyright © lookpolymers.com All Rights Reserved