Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | in-plane, ø25*0.4mm disc; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | in-plane, ø25*0.4mm disc; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 compound |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | in-plane, ø25*0.4mm disc; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 compound |
|||
Thermal Conductivity | 10.0 - 11.0 W/m-K | 69.4 - 76.3 BTU-in/hr-ft²-°F | ASTM C177 |
PolyOne Therma-Tech™ SF-6000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | Through Thickness; ASTM-D5470 Modified (at 110kPa/16 psi/1.1 bar) |
GrafTech eGRAF® HITHERM™ HT-1205 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | Through Thickness; ASTM-D5470 Modified (at 110kPa/16 psi/1.1 bar) |
GrafTech eGRAF® HITHERM™ HT-1210 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | Through Thickness; ASTM-D5470 Modified (at 110kPa/16 psi/1.1 bar) |
GrafTech eGRAF® HITHERM™ HT-1220 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 62 GR/50 PA 6, 50% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 87/28 GR/50 PC, 50% Graphite Reinforced High thermal conductivity product based on Polycarbonate (PC). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 92 GR/65 PUR, 65% Graphite Reinforced High thermal conductivity product based on Polyurethane (PUR). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
Special Metals INCONEL® Alloy G-3 A nickel-chromium-iron alloy with additions of molybdenum and copper. It has good weldability and resistance to intergranular corrosion in the welded condition. The low carbon content helps preven.. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
Special Metals INCONEL® G-3 Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
Special Metals NILO® Alloy 36 Low-Expansion Alloy Inflection point 220°C. A nickel-iron low-expansion alloy containing 36% nickel. It maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coeffic.. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
Cytec Thornel® Graphite Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
Cytec Thornel® Graphite Cloth Laminate with Mil R-9299 Resin Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Thermal Conductivity | 10.0 - 200 W/m-K | 69.4 - 1390 BTU-in/hr-ft²-°F | |
Alliance A-5S Alnico Magnetic Material |
|||
Thermal Conductivity | 10.0 - 200 W/m-K | 69.4 - 1390 BTU-in/hr-ft²-°F | |
Alliance A-8S Alnico Magnetic Material |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
Alliance S-20A Samarium Cobalt Magnetic Material |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
Alliance S-20B Samarium Cobalt Magnetic Material |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
Alliance S-26A Samarium Cobalt Magnetic Material |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
ATI Wah Chang TI-45 Nb Applications: Aerospace Rivet Material; High Pressure Oxygenated Gas Vents; Superconducting Wire Information provided by ATI Wah Chang |
|||
Thermal Conductivity | 10.0 - 200 W/m-K | 69.4 - 1390 BTU-in/hr-ft²-°F | |
Alliance A-6S Alnico Magnetic Material |
|||
Thermal Conductivity | 10.0 - 200 W/m-K | 69.4 - 1390 BTU-in/hr-ft²-°F | |
Alliance A-2S Alnico Magnetic Material |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
Pyrotek Pyrocast SC-2600 Refractory Cast Parts Resistant to metal and flame abrasion, Pyrocast SC-2600 is the recommended castable refractory for applications such as filter box frames, burner tubes and troughs. The high purity silicon carbide .. |
|||
Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
Alliance S-22B Samarium Cobalt Magnetic Material |