Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Laticonther 52/11 CP1/600 F3 PP Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LATI
Trade Name Laticonther
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Laticonther 52/11 CP1/600 F3 PP Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
Linear Mold Shrinkage, Flow 0.0090 - 0.014 cm/cm
0.0090 - 0.014 in/in
Linear Mold Shrinkage, Transverse 0.0090 - 0.014 cm/cm
0.0090 - 0.014 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.0 MPa
3190 psi
Elongation at Break 1.0 %
1.0 %
Tensile Modulus 3.50 GPa
508 ksi
Charpy Impact Unnotched 0.500 J/cm²
2.38 ft-lb/in²
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
Thermal Properties Metric English Comments
Thermal Conductivity 5.00 W/m-K
34.7 BTU-in/hr-ft²-°F
Longitudinal
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
Vicat Softening Point 110 °C

@Load 5.00 kg
230 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Processing Properties Metric English Comments
Melt Temperature 230 - 250 °C
446 - 482 °F
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Drying Temperature 80.0 - 90.0 °C

@Time 10800 sec
176 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved