Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon KOPA® KN135G33HI Multi Reinforced Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Kolon
Trade Name Kopa®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOPA® KN135G33HI Multi Reinforced Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubrication and abrasion resistance, excellent chemical resistance, wide usage temperature, good impact absorbing characteristicsInformation provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
DIN 53479; ASTM D792
Water Absorption 0.40 %
0.40 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
DIN 53505; ASTM D785
Tensile Strength, Ultimate 118 MPa
17100 psi
DIN 53455; ASTM D638
Elongation at Break 5.0 %
5.0 %
DIN 53455; ASTM D638
Flexural Yield Strength 169 MPa
24500 psi
DIN 53455; ASTM D790
Flexural Modulus 5.88 GPa
853 ksi
DIN 53452; ASTM D790
Izod Impact, Notched 1.67 J/cm
3.12 ft-lb/in
DIN 53453; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 220 °C
428 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 190 °C
374 °F
DIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
DIN 53461; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149/DIN 53481
Arc Resistance 135 sec
135 sec
ASTM D495
Users viewing this material also viewed the following: