Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 135 sec | 135 sec | |
Pyrotek TS-235 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Tan color. Highly flexible. High heat resistance.Information provided by Pyrotek. |
|||
Arc Resistance | 135 - 145 sec | 135 - 145 sec | Average value: 138 sec Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Arc Resistance | 135 - 180 sec | 135 - 180 sec | Average value: 164 sec Grade Count:4 |
Overview of materials for Phenolic, Resole, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Kolon KOPA® KN333G15 G/F Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Kolon KOPA® KN333G15SIBL G/F Reinforced Nylon 66 High strength, high toughnessApplications Relay coversInformation provided by API-Kolon. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Kolon KOPA® KN333G30CRN G/F Reinforced Nylon 66 Oil resistantApplications Surge tanksInformation provided by API-Kolon. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Kolon KOPA® KN333G30HS G/F Reinforced Nylon 66 High thermal resistant, high strength, dimensionally stableApplications Transmission gear supportersInformation provided by API-Kolon. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Kolon KOPA® KN333G33BL G/F Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Kolon KOPA® KN333G33CR G/F Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Kolon KOPA® KN333G35CR G/F Reinforced Nylon 66 High thermal resistant, Weather resistant, dimensionally stableApplications Cylinder head coversInformation provided by API-Kolon. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Kolon KOPA® KN333G35CRBK G/F Reinforced Nylon 66 EG-resistant, high strength, dimensionally stableApplications Coolant temperature control partsInformation provided by API-Kolon. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Kolon KOPA® KN333G45 G/F Reinforced Nylon 66 G/F 45% reinforcedApplications Internal gearsInformation provided by API-Kolon. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Haysite HTF Polyester, High Temp Flex HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 3-2-530-P Long-Glass Reinforced Diallyl Phthalate Long glass fiber reinforced, flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 Type GII-30F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 630 Fiberglass Reinforced Phenolic RX 630 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North America. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Sumitomo Bakelite North America 2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Am.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Plenco 2311 Phenolic, Granular, Compression Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Toyobo Vylopet® EMC310K Glass Reinforced Polyester, Easy Molding Grade Key Feature: HB UL-94 classApplications: General componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemic.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Eastman Cadence™ GS3 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Arc Resistance | 135 - 180 sec | 135 - 180 sec | Average value: 144 sec Grade Count:12 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 1-501AN Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Arc Resistance | 135 sec | 135 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 1-510N Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Arc Resistance | 135 sec | 135 sec | |
Cosmic Plastics 6120 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Arc Resistance | 135 sec | 135 sec | |
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |