Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Isoflon Virgin PTFE Polytetrafluoroethylene

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded
Manufacturer Isoflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon Virgin PTFE Polytetrafluoroethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties/Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityExcellent resistance to continuous service temperatures up to 260°C, and, for limited periods, even to higher temperaturesChemical resistance: PTFE possesses a high inertness towards nearly all known chemicals. It is only attacked by elemental alkali metals, chlorine trifluoride and elemental fluorine at high temperatures and pressures.Solvents resistance: PTFE is insoluble in all solvents up to temperatures as high as 300°C. Certain highly fluorinated oils only swell and dissolve PTFE close to the crystalline melting point.Information provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 2.13 - 2.18 g/cc
2.13 - 2.18 g/cc
ISO 1183
Water Absorption 0.0010 %
0.0010 %
ASTM D570
Deformation 6.0 - 7.5 %

@Time 86400 sec
6.0 - 7.5 %

@Time 24.0 hour
After relaxation period; ASTM D695
10 - 13 %

@Time 86400 sec,
Pressure 13.7 MPa
10 - 13 %

@Time 24.0 hour,
Pressure 1990 psi
Under load; ASTM D695
Mechanical Properties Metric English Comments
Hardness, Shore D 54 - 60
54 - 60
ISO 868
Tensile Strength 20.0 - 30.0 MPa
2900 - 4350 psi
ISO 527
Elongation at Break 200 - 300 %
200 - 300 %
ISO 527
Flexural Modulus 0.600 - 0.700 GPa
87.0 - 102 ksi
Coefficient of Friction, Dynamic 0.070
0.070
ASTM D1894
Thermal Properties Metric English Comments
Melting Point 325 - 335 °C
617 - 635 °F
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
Minimum Service Temperature, Air -200 °C
-328 °F
Continuous
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D 257
Dielectric Constant 2.1

@Frequency 6.00e+7 - 2.00e+9 Hz
2.1

@Frequency 6.00e+7 - 2.00e+9 Hz
ASTM D150
Dielectric Strength 20.0 - 70.0 kV/mm
508 - 1780 kV/in
ASTM D149
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved