Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.13 - 2.23 g/cc | 2.13 - 2.23 g/cc | ASTM D1457-18; ISO.1183 DN.53479 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Specific Gravity | 2.13 - 2.23 g/cc | 2.13 - 2.23 g/cc | ASTM D1457-18; ISO.1183 DN.53479 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Specific Gravity | 2.13 - 2.18 g/cc | 2.13 - 2.18 g/cc | ISO 1183 |
Isoflon Virgin PTFE Polytetrafluoroethylene Properties/Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityExcellent resistance to continuous service temperatures up to 260°C, and, for limited per.. |
|||
Specific Gravity | 2.13 - 2.18 g/cc | 2.13 - 2.18 g/cc | ISO 12086 |
Isoflon PTFE Polytetrafluoroethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Specific Gravity | 2.13 g/cc | 2.13 g/cc | ASTM D297, 15 |
Seals Eastern Perflas® 9294 Perfluorinated Rubber Perfluoro rubber for aggressive chemical service. Perflas ® 9294 seals are made of a chemical resistant perfluorinated fluoroelastomer (FFKM). Perflas 9294 seals offer outstanding resistance to.. |
|||
Specific Gravity | 2.13 - 2.16 g/cc | 2.13 - 2.16 g/cc | |
Shandong Dongyue Polymer DF-17 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as the packing products resource and packing pelletized resource, which can be processed to film, the products of thin wall, seal, gasket, club, panel, tube, axletree.. |
|||
Specific Gravity | 2.13 g/cc | 2.13 g/cc | ASTM-D792 |
CoorsTek PolyGlyde™ 2000 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON F-201 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON F-302 PTFE Fine Powder Processing Methods: Paste extrusion.Applications: Small to large diameter tubes, flexible hoses, shrinkable tubes, heavy duty electric wires smaller than AGW18, and jackets.Information provided by .. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON M-18 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Suited to molding of large billets, has nearly the same molding characteristics of M-12. Also allows uniform mixing of inorganic fi.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder 15% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1040 PTFE 20% Glass Fiber Filled Molding Powder 20% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1040F PTFE 20% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 20% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1050F PTFE 25% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 25% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1241 PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder 20% glass fiber and 5% graphite filled. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (e.g. piston rings, bearing pads, and packings)Inform.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1241F PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder, High Apparent Density, Free Flow 20% glass fiber and 5% graphite filled. High apparent density and free-flowing properties. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1431 PTFE 15% Glass Fiber and 5% MoS2 Filled Molding Powder 15% glass fiber and 5% MoS2 filled. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanical and electrical service (e.g. split-curled bearings.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow 15% glass fiber and 5% MoS2 filled. High apparent density and free-flowing properties. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanica.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder 15% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-6030 PTFE 15% Carbon Fiber Filled Molding Powder 15% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by .. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-6030F PTFE 15% Carbon Fiber Filled Molding Powder, High Apparent Density, Free Flow 15% carbon fiber filled. High apparent density and free-flowing properties. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechan.. |
|||
Specific Gravity | 2.13 g/cc | 2.13 g/cc | |
Epoxy Technology EPO-TEK® H31D-LV Epoxy Material Description: A single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and optoelectronic packaging. It i.. |
|||
Specific Gravity | 2.13 - 2.22 g/cc | 2.13 - 2.22 g/cc | ASTM D792 |
Daikin POLYFLON MG-1050 PTFE 25% Glass Fiber Filled Molding Powder 25% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |