Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 325 °C | 617 °F | ASTM D570 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Melting Point | 325 °C | 617 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
Melting Point | 325 - 330 °C | 617 - 626 °F | ISO.3146 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Melting Point | 325 - 330 °C | 617 - 626 °F | ISO.3146 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Melting Point | 325 - 330 °C | 617 - 626 °F | |
Solvay Specialty Polymers Polymist® F-5A EX PTFE Powder Lubricant
(Unverified Data**) Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist .. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L203F Polytetrafluoroethylene (PTFE) Algoflon® L203F a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L203F can be de-agglomerat.. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L206 Polytetrafluoroethylene (PTFE) Algoflon® L206 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L206 can be de-agglomerated.. |
|||
Melting Point | 325 °C | 617 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AE-8930 Polyphthalamide (PPA), 30% Glass Fiber Amodel® AE-8930 is a 30% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Melting Point | 325 - 335 °C | 617 - 635 °F | ASTM D3418 |
Solvay Specialty Polymers Algoflon® L203 Polytetrafluoroethylene (PTFE) Algoflon® L203 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L203 can be de-agglomerated.. |
|||
Melting Point | 325 °C | 617 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo.. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HTM-4H1 PA6T/6I-MD40 Product description: Grivory HTM-4H1 is a 40 % mineral reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA .. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30 Product description: Grivory HTV-3H1 black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45 Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a.. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40 Product description: Grivory HTV-4H1 natural is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HTV-6H1 nat PA6T/6I-GF60 Product description: Grivory HTV-6H1 natural is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Melting Point | 325 °C | 617 °F | ISO 3146 |
ExxonMobil PP8013L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with very high impact strength at low temperature. It is suitable for molding applications like containers and tubs, other rigid packaging, t.. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT1V-3 FWA black 9225 PA6T/6I-GF30 Product description: Grivory HT1V-3 FWA black 9225 is a 30 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT1V-3 FWA nat PA6T/6I-GF30 Product description: Grivory HT1V-3 FWA natural is a 30 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA natural is a 50 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Melting Point | 325 °C | 617 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65 Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I.. |
|||
Melting Point | 325 °C | 617 °F | Peak Temperature |
3M Dyneon™ TF 9205 PTFE 3M™ Dyneon™ PTFE TF micropowders can be used as additives in many different applications and at concentrations typically from 5 to 20%. Homogeneous incorporation helps ensure optimum performance. .. |
|||
Melting Point | 325 °C | 617 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)
(discontinued **) Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, .. |