Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 70.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 11.0 - 70.0 kV/mm
280 - 1780 kV/in
Average value: 27.9 kV/mm Grade Count:55
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Dielectric Strength 13.0 - 70.0 kV/mm
330 - 1780 kV/in
Average value: 26.1 kV/mm Grade Count:52
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Dielectric Strength 20.0 - 70.0 kV/mm
508 - 1780 kV/in
ASTM D149
Isoflon Virgin PTFE Polytetrafluoroethylene
Properties/Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityExcellent resistance to continuous service temperatures up to 260°C, and, for limited per..
Dielectric Strength 20.0 - 70.0 kV/mm
508 - 1780 kV/in
DIN 53481
Isoflon PTFE Polytetrafluoroethylene
Fluoropolymer material specifications.Information provided by Isoflon.
Dielectric Strength 20.0 - 70.0 kV/mm
508 - 1780 kV/in
ASTM D149
Adamas Adalon® 991 PTFE
Information provided by Adamas, HPM
Dielectric Strength 20.0 - 70.0 kV/mm
508 - 1780 kV/in
ASTM D149
Adamas Adalon® 998 PTFE, Turquoise
Information provided by Adamas, HPM
Dielectric Strength 20.0 - 70.0 kV/mm
508 - 1780 kV/in
ASTM D149
Adamas Adalon® 451 PTFE, organic filler
Information provided by Adamas, HPM
Dielectric Strength 16.5 - 70.0 kV/mm
420 - 1780 kV/in
Average value: 32.8 kV/mm Grade Count:8
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Dielectric Strength 50.0 - 70.0 kV/mm
1270 - 1780 kV/in
DIN 53481
Isoflon PCTFE Polychlorotrifluoroethylene
Fluoropolymer material specifications.Information provided by Isoflon.
Dielectric Strength 20.0 - 70.0 kV/mm
508 - 1780 kV/in
ASTM D149
Adamas Adalon® 911 PTFE
Information provided by Adamas, HPM
Copyright © lookpolymers.com All Rights Reserved