Mechanical Properties Metric English Comments
Tensile Strength 20.0 - 30.0 MPa
2900 - 4350 psi
Injection; ISO 527
Raschig Group 4554 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi..
Tensile Strength 25.0 - 30.0 MPa
3630 - 4350 psi
DIN 53288
Permabond TA439 Toughened Acrylic Adhesive
Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f..
Tensile Strength 20.0 - 30.0 MPa

@Temperature 25.0 °C
2900 - 4350 psi

@Temperature 77.0 °F
stainless steel after 24 hours
Permabond TA459 Toughened Acrylic Adhesive
Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens..
Tensile Strength 20.0 - 30.0 MPa

@Temperature 25.0 °C
2900 - 4350 psi

@Temperature 77.0 °F
stainless steel after 24 hours
Permabond TA4590 Toughened Acrylic Adhesive
Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen..
Tensile Strength 25.0 - 30.0 MPa
3630 - 4350 psi
DIN 53455
Isoflon PFA Polyperfluoroalkoxyethylene
Fluoropolymer material specifications.Information provided by Isoflon.
Tensile Strength 20.0 - 30.0 MPa
2900 - 4350 psi
ISO 527
Isoflon Virgin PTFE Polytetrafluoroethylene
Properties/Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityExcellent resistance to continuous service temperatures up to 260°C, and, for limited per..
Tensile Strength 20.0 - 30.0 MPa
2900 - 4350 psi
DIN 53455
Isoflon PTFE Polytetrafluoroethylene