Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos K44-15-122 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos K44-15-122 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
K44-15-122 is a natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF Standard 61 health effects requirements, and is recognized by the Plastic Pipe Institute as having a pipe material designation code of PE 3608 (formerly PE 3408). A pressure rated formulation is also produced when this product is extruded in combination with a Ineos approved black masterbatch. The resulting formulation known as K44-15-123 has NSF Standard 14 certification and complies with ANSI/NSF Standard 61 health effects requirements, is certified to CSA Standard B137.1-05 and B137.4-05, and is listed with the Plastic Pipe Institute as a PE 3608(formerly PE 3408) and PE 80 pipe material designation code.
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
Natural; ASTM D4883
Environmental Stress Crack Resistance >= 2000 hour
>= 2000 hour
Condition B; ASTM D1693
>= 5000 hour
>= 5000 hour
Condition C; ASTM D1693
High Load Melt Index 12.5 g/10 min
12.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
PENT >= 100 hour
>= 100 hour
Notch Tensile; ASTM F1473
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength at Break 31.0 MPa
4500 psi
2 in/min.; ASTM D638
Tensile Strength, Yield 22.8 MPa
3310 psi
2 in/min.; ASTM D638
Elongation at Break >= 800 %
>= 800 %
2 in/min.; ASTM D638
Flexural Modulus 0.827 GPa
120 ksi
2% Secant-Method 1; ASTM D790
Izod Impact, Notched 3.20 J/cm
5.99 ft-lb/in
ASTM D256
Hydrostatic Design Basis 11.0 MPa
1600 psi
ASTM D2837
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Brittleness Temperature <= -118 °C
<= -180 °F
ASTM D746
Descriptive Properties Value Comments
Process Color Concentrate
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: