Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 12.5 g/10 min | 12.5 g/10 min | ASTM D1238 |
Ineos K44-15-122 HDPE K44-15-122 is a natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF S.. |