Solvay Chemicals CASO® FCC FLAKES Food Additive INS 509, Calcium Chloride

Category Ceramic , Halide
Manufacturer Solvay Chemicals
Trade Name CASO®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals CASO® FCC FLAKES Food Additive INS 509, Calcium Chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CASO® FCC Flakes is a dihydrate calcium chloride food grade of mineral origin. According to the International Numbering System (INS) for food additives, CASO® FCC Flakes is characterized by the INS Number 509 referring to "calcium chloride". CASO® FCC Flakes is compatible with the food uses for which the Food Chemicals Codex (8th Edition) specifications are required, but does not constitute a food additive pursuant to European Regulation N° 1333/2008 as amended. REACH Registration Number: 01-2119494219-28/ CAS number: 10035-04-8/ EINECS - N°: 233-140-8/ CE - N°: 017-013-00-2 Applications: Agriculture, Dairy products and cheese, Production of beer and soft drinks, Storage of canned fruits and vegetables, Cooling agent in food processes and Food AdditiveInformation provided by Solvay
Physical Properties Metric English Comments
Density 0.800 - 0.900 g/cc
0.0289 - 0.0325 lb/in³
Molecular Weight 147.02 g/mol
147.02 g/mol
Descriptive Properties Value Comments
Appearance Flakes
Color White
Composition <0.004%
Fluorides
<0.004%
Fluorides, Specifications
<1 mg/kg
Hg
<1 mg/kg
Hg, Specifications
<1.5 g/kg
Ca(OH)2, Specifications
<3 mg/kg
As
<3 mg/kg
As, Specifications
<40 g/kg
Magnesium and alkali salts, Specifications
<5 mg/kg
Pb, Specifications
0.7 g/kg
Water insoluble
0.9 g/kg
Ca(OH)2
1.02
CaCl2.2H2 O
1.6 g/kg
SO4
1.6 mg/kg
Pb
10.2
pH of 1:20 solution
26 g/kg
Magnesium and alkali salts
26 g/kg
NaCl
4.5-11
pH of 1:20 solution, Specifications
4.7 mg/kg
Fe
750-810 g/kg
CaCl2, Specifications
770 g/kg
CaCl2
99-107%
CaCl2.2H2 O, Specifications
Granulometry 0.014
<0.5 mm, statistical average
0.018
<1.0 mm, statistical average
0.055
<2.0 mm, statistical average
0.06
<0.5 mm, typical value
0.08
<1.0 mm, typical value
0.27
<2.0 mm, typical value
0.493
<4.0 mm, statistical average
0.83
<4.0 mm, typical value
0.983
<8.0 mm, statistical average
1
<8.0 mm, typical value