Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | F20, Condition C, ASTM D1693, 100% Igepal |
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provid.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | F0, Condition C, ASTM D1693, 100% Igepal |
NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | F0, Condition C, ASTM D1693, 100% Igepal |
NOVA Chemicals Novapol® HD-2100-A MDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | No failures; ASTM D 1693 cond. C |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | No failures; ASTM D 1693 cond. C |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour @Temperature 50.0 °C |
>= 5000 hour @Temperature 122 °F |
Conditions A, B and C; ASTM D 1693 |
Chevron Phillips Marlex® HHM TR-418N/M358Y Natural medium density ethylene hexene copolymer/yellow concrete
( Benefits: environmentally-friendly pigment system, yellow color for easy identification, outstanding pipe rind ESCR, UV stabilizer in natural resin, concentrate base resinCharacteristics: Pipe Ring .. |
|||
Environmental Stress Crack Resistance | 5000 hour | 5000 hour | > 5000 hrs.; ASTM D1693 |
Ineos K38-20-160 Polyethylene Copolymer K38-20-160 is a medium density polyethylene copolymer containing an organic yellow pigment system, designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stres.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition B; 10%; ASTM D1693 |
Ineos K38-20-188 HDPE K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural .. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition C; ASTM D1693 |
Ineos K38-20-188 HDPE K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural .. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Pipe Ring; ASTM F1248 |
Ineos K38-20-188 HDPE K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural .. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | ASTM D 1693 |
Ineos K38-20X2091 HDPE K38-20X2091 is a yellow medium density polyethylene resin designed specifically for natural gas pipe extrusion. It exhibits excellent long term stress life and slow crack growth resistance. This m.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | ASTM F 1248 |
Ineos K38-20X2091 HDPE K38-20X2091 is a yellow medium density polyethylene resin designed specifically for natural gas pipe extrusion. It exhibits excellent long term stress life and slow crack growth resistance. This m.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | ASTM D 1693 |
Ineos K38-20X2091 HDPE K38-20X2091 is a yellow medium density polyethylene resin designed specifically for natural gas pipe extrusion. It exhibits excellent long term stress life and slow crack growth resistance. This m.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition C; ASTM D 1693 |
Ineos K44-08-123 HDPE Copolymer with Carbon Black Fortiflex® K44-08-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition C; ASTM D1693 |
Ineos K44-15-122 HDPE K44-15-122 is a natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF S.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition C; same value for Pipe Ring ESCR; ASTM D 1693 |
Ineos K44-15-123 HDPE Copolymer with Carbon Black Fortiflex® K44-15-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition C; ASTM D1693 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. .. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition C; ASTM D1693 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. I.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition C; ASTM D1693 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition C; ASTM D1693 |
Ineos TUB 121 HDPE TUB 121 (aka ELTEX® TUB 121, ELTEX® TUB 121 N2025, and ELTEX® TUB 121 N3000) is a black high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, ind.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition C; ASTM D1693 |
Ineos TUB 121N HDPE TUB121N is a natural high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, industrial, and mining pipe. When blended with an approved black concentrate, t.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition C; ASTM D1693 |
Ineos TUB 121NTW HDPE TUB121 NTW is a natural high density bimodal polyethylene copolymer designed for extrusion of large diameter, thick wall piping for potable water, industrial and mining applications. When blended wi.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition C; ASTM D1693 |
Ineos K44-08-122 HDPE K44-08-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as havin.. |
|||
Environmental Stress Crack Resistance | <= 5000 hour | <= 5000 hour | F50; ASTM D1693 |
CPC - Vycom HITEC® HDPE High Density Polyethylene Hitec HDPE is a high impact, high density polyethylene sheet. It is ideally suited for the manufacture of chemical resistant products which come in direct contact with foodstuffs. Hitec meets the st.. |
|||
Environmental Stress Crack Resistance | <= 5000 hour | <= 5000 hour | F50; ASTM D2561 |
CPC - Vycom HITEC® HDPE High Density Polyethylene Hitec HDPE is a high impact, high density polyethylene sheet. It is ideally suited for the manufacture of chemical resistant products which come in direct contact with foodstuffs. Hitec meets the st.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | ASTM D1693 cond. B 100% lgepal |
Total Finathene® 4344 HDPE, blow molding
(discontinued **) Applications: storage tank liners, intermediate bulk containers, general large-part blow molding. Blow Molding Stock Temperature 370 – 410 ºFInformation provided provided by Total Petrochemicals.T.. |
|||
Environmental Stress Crack Resistance | >= 5000 hour | >= 5000 hour | Condition A,B,C (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HP3902 Pipe HDPE Natural Medium Density Hexene CopolymerApplications: Pipe for gas distribution, oilfield and other industrial pipe, telecommunications conduit.Formolene HP3902 is a high performance copolymer that i.. |