Mechanical Properties | Metric | English | Comments |
---|---|---|---|
PENT | >= 100 hour | >= 100 hour | Slow Crack Growth; ASTM F1473 |
Polymer Industries Densetec HDPE Pipe Grade The material displays improved performance characteristics in a variety of piping applications. In addition the material is UV stabilized and ideal for use in demanding outdoor applications. It reta.. |
|||
PENT | >= 100 hour | >= 100 hour | ASTM F1473 |
Petromont DGDP-2485 High Density Polyethylene Resin Pétromont® DGDP-2485 Natural is a high density polyethylene copolymer produced using the UNIPOL® process technology. DGDP-2485 is a high performance resin with very high melt strength, excellent .. |
|||
PENT | >= 100 hour | >= 100 hour | Slow crack growth; ASTM F1473 |
Chevron Phillips Marlex® HHM TR-480X HDPE Pipe and Corrugated Extrusion Resin
(discontinued **) Characteristics: Good long-term hoop strength performanceVery high melt strengthOutstanding low temperature toughnessApplications: Municipal, industrial, and mining pipeOil and gas gathering pipeInf.. |
|||
PENT | >= 100 hour | >= 100 hour | Slow crack growth; ASTM F1473 |
Chevron Phillips Marlex® HHM TR-480XC HDPE Pipe and Corrugated Extrusion Resin
(discontinued **) Characteristics: Good long-term hoop strength performanceVery high melt strength>Outstanding low temperature toughnessApplications: Municipal, industrial, and mining pipeOil and gas gathering pipeIn.. |
|||
PENT | >= 100 hour | >= 100 hour | Notch Tensile; ASTM F1473 |
Ineos K44-15-122 HDPE K44-15-122 is a natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF S.. |
|||
PENT | >= 100 hour | >= 100 hour | Notch Tensile; ASTM F1473 |
Ineos K44-06-122 HDPE HDPE K44-06-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as .. |
|||
PENT | >= 100 hour | >= 100 hour | Notch Tensile; ASTM F1473 |
Ineos K44-08-122 HDPE K44-08-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as havin.. |
|||
PENT | >= 100 hour | >= 100 hour | ASTM F 1473 |
Total HP 401N Natural HDPE, pipe Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by T.. |