Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.8 MPa | 3310 psi | ASTM D638 |
Resirene Resirene® 6220 High Impact Polystyrene Features:Low FlowEasy ProcessingGood GlossHigh ElongationFDA Rating: 21 CFR 177.1640Mechanical StrengthApplications:Extrusion/ ThermoformingDisposablesGPPS/HIPS BlendsRefrigerator PartsInformation p.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | 150x10x4 mm specimen, 50 mm/min; ASTM D638 |
Solvay Engineered Polymers INDURE™ X190 TPO
(discontinued **) Description: INDURE™ X190 engineered polyolefin material is designed for large, molded-in-color automotive exterior applications that require good scratch and mar characteristics, high stiffness, a.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | ASTM D638 |
Chevron Phillips HiD® 9062 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | Crosshead speed - 2" min; ASTM D638 |
LyondellBasell Alathon® M4661 High Density Polyethylene ApplicationsALATHON M 4661, formerly known as LYHD 060, exhibits excellent impact, warp and environmental stress crack resistance. Typical applications are closures, institutional seating and consum.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | 2 in/min.; ASTM D638 |
Ineos K44-15-122 HDPE K44-15-122 is a natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF S.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | ASTM D638 |
Ineos K44-15-123 HDPE Copolymer with Carbon Black Fortiflex® K44-15-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | 2 in/min (50 mm/min); ASTM D638 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Tensile Strength, Yield | 22.8 MPa @Temperature 23.0 °C |
3310 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Polene HI650 Polystyrene APPLICATIONS: INJECTION MOULDING, ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY WARES. etc. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | 2 in/min.; ASTM D638 |
Ineos K44-08-122 HDPE K44-08-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as havin.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | 2 in/min; ASTM D638 |
ExxonMobil PP7035E4 Impact Copolymer Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional .. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | ASTM D638 |
Dow C702-20NA Polypropylene Impact Copolymer Resin OverviewHigh impact performanceContains a nucleating additiveContains an antistatic additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C702-20NA Polypropylene Resin is intended f.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® SMR1000 Thermoplastic Polyolefin Elastomer Elastocon® SMR1000 thermoplastic polyolefin elastomer has been developed for applications that require impact resistance and a high gloss scratch and mar resistant surface finish. Elastocon® SMR10.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | ASTM D412 |
ACC EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea EP RAP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Aliphatic Polyurea (silicone optional) that has excellent UV stability (colorfast) with supe.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | ASTM D412 |
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3310 psi | 2.0 in/min; ASTM D638 |
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |