Polymer Property : Flexural Modulus = 0.827 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.827 GPa
120 ksi
Tangent; ASTM D790
RheTech Products FT1003-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step and hitch padsInterior component and trimA/B pillarsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 0.827 GPa
120 ksi
Tangent; ASTM D790
RheTech Products FT2600-677UV Thermoplastic Polyolefin, UV Stabilized, 0848 Black
Applications: Exterior trimStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
PolyOne Maxxam™ FR MF5210-0301 DK GRAY 2451 Polypropylene, Unspecified (PP, Unspecified)
Information provided by PolyOne
Flexural Modulus 0.827 GPa
120 ksi
ASTM D 790
RTP Company RTP 700 High Density Polyethylene (HDPE), Unfilled
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
ExxonMobil Escorene® HD-6908 HDPE, Injection Grade  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Excellent Stiffness, Good ImpactUses: Crates, Pails, Industrial containers
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Honeywell Aegis™ PL165HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer  (discontinued **)
Description: Aegis PL165HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt ..
Flexural Modulus 0.827 GPa
120 ksi
Tangent; ASTM D790
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
LTL Color Compounds ColorRxâ„¢ PP2-1001A Antimicrobial Polypropylene Random Copolymer
An approx. 10 melt Polypropylene random copolymer containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL ..
Flexural Modulus 0.827 GPa
120 ksi
2% Secant-Method 1; ASTM D790
Ineos K44-08-122 HDPE
K44-08-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as havin..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D882
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D882
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
Flexural Modulus 0.827 GPa
120 ksi
2% secant; ASTM D790
A. Schulman LP544-01 High-Density Copolymer Polyethylene
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Westlake Plastics Propylux® Polypropylene
Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance it abrasion. These properties makes it suitable f..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D 790
RTP Company RTP 1500-72D TFE 15 Polyether-Ester Block Copolymer (TEEE / COPE), PTFE Lubricated - Preliminary Data
Flexural Modulus 0.827 GPa
120 ksi
ASTM D 790
RTP Company RTP 154 HI Polypropylene (PP), Copolymer - Flame Retardant
The RTP 154 family of compounds are flame retarded, unreinforced polypropylene materials. They offer improved physical properties, low specific gravity and excellent moldability vs. traditional V-0..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D 790
RTP Company RTP 199 X 137777 C Polypropylene (PP) Co-Polymer - High Flow - High Impact - Flame Retardant - UV Stabilized
Flexural Modulus 0.827 GPa
120 ksi
1% secant; ASTM D790
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D882
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Eastman Tenite 485E3720023 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Flexural Modulus 0.827 GPa
120 ksi
0.05 in/min; ISO 178
CTC X-PRO CTC PP 3020 Polypropylene Copolymer
X-PRO PP 3020 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Diamond Polymers NPP11-0242 Polyethylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 0.827 GPa
120 ksi
Dow DOWLEX™ IP-22 High Density Polyethylene
DOWLEX® IP-22 resin is an improved processing high density polyethylene resin designed for excellent flow, high impact, and moderate stiffness. DOWLEX IP-22 resin balances peak molecular weight wit..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D882
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
Flexural Modulus 0.827 GPa
120 ksi
1.3mm per min, 1% secant; ASTM D790
Formosa Plastics Formolene® 2706A Injection Molding RTPO Polypropylene  (discontinued **)
Reactor (In-Situ) Thermoplastic Olefin (RTPO)Applications: Automotive, appliances, lawn and garden, medical and rigid packaging.Formolene 2706A is an RTPO made with the latest gas phase technology c..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D 790
RTP Company RTP 2800 B-65DZ Thermoplastic Polyolefin Elastomer (TEO) - FDA Compliant Ingredients  (discontinue
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Flexural Modulus 0.827 GPa
120 ksi
ASTM D 790
RTP Company ESD A 100 Polypropylene (PP), ESD Protection - Static Dissipative - Standard (Low) MFR
Flexural Modulus 0.827 GPa
120 ksi
ASTM D 790
RTP Company RTP 3199 X 117877 B Perfluoroalkoxy (PFA), Carbon Nanotube - Electrically Conductive - High Purity
Flexural Modulus 0.827 GPa
120 ksi
1.3mm per min, 1% secant; ASTM D790
Formosa Plastics Formolene® 2620A Impact Copolymer Polypropylene
Impact Copolymer for Compounding and Injection Molded Applications Formolene® 2620A is a high impact copolymer of polypropylene designed for applications such as automotive compounds and lawn & gar..