Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 2000 hour @Temperature 50.0 °C |
>= 2000 hour @Temperature 122 °F |
F<sub>50</sub>, Cond. B.; ASTM D1693 |
Chevron Phillips 7105T LLDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 214, A 35307Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour @Temperature 50.0 °C |
>= 2000 hour @Temperature 122 °F |
F<sub>50</sub>, Cond. B.; ASTM D1693 |
Chevron Phillips 7108T LLDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 214, A 35307Applications:Cast Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Containm.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour @Temperature 50.0 °C |
>= 2000 hour @Temperature 122 °F |
Condition A and Condition B; ASTM D 1693 |
Chevron Phillips Marlex® C579 High density polyethylene
(discontinued **) Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceApplications: multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containersInformation pro.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour @Temperature 50.0 °C |
>= 2000 hour @Temperature 122 °F |
Condition A and Condition B; ASTM D 1693 |
Chevron Phillips Marlex® C513 High density polyethylene
(discontinued **) Benefits: outstanding impact and creep resistance, outstanding ESCR, excellent processabilityApplications: intermediate bulk containers, agricultural containersInformation provided by Chevron Philli.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour @Temperature 50.0 °C |
>= 2000 hour @Temperature 122 °F |
F<sub>50</sub>, Cond. B.; ASTM D1693 |
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour @Temperature 50.0 °C |
>= 2000 hour @Temperature 122 °F |
F<sub>50</sub>, Cond. B.; ASTM D1693 |
Chevron Phillips HiD® 9642 HDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour | >= 2000 hour | Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HL4506 Blow Molding HDPE
(discontinued **) Extra High Molecular Weight Hexene CopolymerApplications: Multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containers (IBC)Formolene HL4506 is intended for large part blow molding appl.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour | >= 2000 hour | Condition B (10% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HL4506 Blow Molding HDPE
(discontinued **) Extra High Molecular Weight Hexene CopolymerApplications: Multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containers (IBC)Formolene HL4506 is intended for large part blow molding appl.. |
|||
Environmental Stress Crack Resistance | 2000 hour | 2000 hour | ASTM D1693 |
Global MB-6366 High Density Polyethylene Description-high density for high quality, excellent creep & chemical resistanceApplications-drinking water pipe, industrial pipe, sewer pipeInformation provided by Global Polymers Corporation. |
|||
Environmental Stress Crack Resistance | >= 2000 hour | >= 2000 hour | Condition B; ASTM D1693 |
Ineos K44-15-122 HDPE K44-15-122 is a natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF S.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour | >= 2000 hour | Condition B, 10%; ASTM D1693 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. .. |
|||
Environmental Stress Crack Resistance | >= 2000 hour | >= 2000 hour | Condition B, 10%; ASTM D1693 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. I.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour | >= 2000 hour | ASTM D1693 |
LG Chemical LUTENE CCO550BK PE Compound Description: LUTENE CC0550BK offer the following properties: high mechanical properties, good environmental stress cracking resistance, excellent wetherability and high speed extrusion to give a smo.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour @Temperature 80.0 °C |
>= 2000 hour @Temperature 176 °F |
At 8.0 bar; ISO 13479 |
Borealis Borstar® HE3470-LS Black HDPE Compound for Pressure Pipes Borstar HE3470-LS is a black, high density polyethylene compound classified as an MRS 8.0 material (PE80) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding .. |
|||
Environmental Stress Crack Resistance | >= 2000 hour @Temperature 80.0 °C |
>= 2000 hour @Temperature 176 °F |
At 8 bar; ISO 13479 |
Borealis Borstar® ME3441 Yellow Medium Density Polyethylene for Natural Gas Pipes Borstar ME3441 is a yellow, bimodal, cadmium free, medium density polyethylene compound classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. It includes a combinat.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour | >= 2000 hour | F<sub>o</sub>; Compression molded parts prepared according to ASTM D 1928, condition A.; ASTM D1693 |
Dow DFDC-7525 NT High Density Polyethylene Resin DOW DFDC-7525 NT is produced using UNIPOL™ process technology. It is intended for use in thin wall drip tape and micro-irrigation tube, hose and tube, and profile extrusion applications. Informati.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour @Temperature 50.0 - 50.0 °C |
>= 2000 hour @Temperature 122 - 122 °F |
Average value: 2000 hour Grade Count:2 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Sheeting Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Sheeting Grade". Each property range of values reported is mini.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour @Temperature 80.0 - 80.0 °C |
>= 2000 hour @Temperature 176 - 176 °F |
Average value: 2000 hour Grade Count:2 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour | >= 2000 hour | F<sub>0</sub>; ASTM D1693/B |
Petromont 7002 Medium Density Polyethylene Resin Petromont HDPE 7002 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusi.. |
|||
Environmental Stress Crack Resistance | >= 2000 hour @Temperature 80.0 °C |
>= 2000 hour @Temperature 176 °F |
At 8 bar; ISO 13479 |
Borealis Borstar® ME3444 Blue Medium Density Polyethylene for Drinking Water Pipes Borstar 3444 is a blue, bimodal, medium density polyethylene classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. A combination of pigments and stabilizers is incl.. |