Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IRPC Polimaxx Polene GG3245 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene GG3245 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: EXCELLENT ENVIRONMENTAL STRESS CRACKING RESISTANCE (ESCR) EXCELLENT IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH TOUGHNESSAPPLICATIONS: BLOW MOLDING/ SHEET/ THERMOFORMING EXTRUSION CONTAINERS 5 - 60 LITRES FOR DETERGENT AND INDUSTRIAL CHEMICALS, AUTOPARTS
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
Condition B, F50; ASTM D1693
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
0.25 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
DIN 53505
Tensile Strength at Break 42.0 MPa
6090 psi
ASTM D638
Tensile Strength, Yield 23.5 MPa
3410 psi
ASTM D638
Elongation at Break 1750 %
1750 %
ASTM D638
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 200 - 220 °C
392 - 428 °F