Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
Polimeri Europa Sinkral® B 532/E ABS Resin Sinkral B 532/E is an extrusion grade, which combines high toughness with good rigidity. Its rheological characteristics and good thermal stability are required for the production of large extruded .. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® MG34LGHF ABS Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® XHT1141 PC XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANMID 6 B33^ E F15 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® XHT1141 PC (Europe-Africa-Middle East) XHT1141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | DIN 53453 |
IRPC Polimaxx Polene GG3245 High Density Polyethylene CHARACTERISTICS: EXCELLENT ENVIRONMENTAL STRESS CRACKING RESISTANCE (ESCR) EXCELLENT IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH TOUGHNESSAPPLICATIONS: BLOW MOLDING/ SHEET/ THERMOFORMING EXTRUSION CO.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Triax® 1120 ABS + Polyamide Blend (Conditioned) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Triax® 1120 ABS + Polyamide Blend (DAM) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, Conditioned Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO Data |
Styron Magnum™ SPD 214 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, Conditioned Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30 Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40 Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179-2 |
Denka TE-10 Transparent Resin Polymer (MABS resin) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® HTN 53G50LWSF BK702A Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -40.0 °C |
7.61 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
Dry; ISO 179/Af |
Arkema Group Orgalloy® RS 6000 Polyamide 6 Alloy Polyamide Alloy, Rigid grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® RS 6620 Polyamide 6.6 Alloy 20% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | EN ISO 179 |
Brandenburger BL 20/1 GG EP Rotor Blade Material BL 20/1 GG EP is a composite bearing material that combines the crucial parameters for rotary blades. These include compressive stability at high temperatures, impact strength, low swelling and low.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl A2 ZV40 Nylon 66, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 (2500) PA 6 Conditioned AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | Wet |
Asahi Kasei Leona® 1300G Polyamide 66 Resin, Glass Reinforced Applications: Automotive: Radiator Tanks, Fuel Injectors, ABS Sensors, Engine Mounts Electrical and Industrial: Heater Tanks, Office Furniture, Small EnginesInformation provided by Asahi Kasei |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 30.0 °C |
7.61 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril.. |
|||
Charpy Impact, Notched | 1.60 - 3.20 J/cm² | 7.61 - 15.2 ft-lb/in² | Average value: 2.22 J/cm² Grade Count:9 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma.. |