Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® BC 82 High Density Polyethylene - Blow Molding Eraclene BC 82 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er.. |
|||
Melt Flow | 0.25 - 0.40 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 - 0.40 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.25 - 0.40 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 - 0.40 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6152C (526H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.25 - 0.40 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 - 0.40 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6948C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.25 - 0.40 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 - 0.40 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6949C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.25 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene AM3245 PC High Density Polyethylene CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS: PIPE EXTRUSIONSU.. |
|||
Melt Flow | 0.25 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene GA3245 High Density Polyethylene CHARACTERISTICS: HIGH TOUGHNESS, GOOD EXTRUDABILITY, EXCELLENT IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR CARRIER BAGS, GROCERY BAGS, SHOPPING BAGS, INDUSTRIAL BAGS, LINER BAGS |
|||
Melt Flow | 0.25 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene GA3750 High Density Polyethylene CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS |
|||
Melt Flow | 0.25 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene GA3750 High Density Polyethylene CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS |
|||
Melt Flow | 0.25 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene GG3245 High Density Polyethylene CHARACTERISTICS: EXCELLENT ENVIRONMENTAL STRESS CRACKING RESISTANCE (ESCR) EXCELLENT IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH TOUGHNESSAPPLICATIONS: BLOW MOLDING/ SHEET/ THERMOFORMING EXTRUSION CO.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE HD 7800P High Density Polyethylene Copolymer Resin Product Description: HD 7800P is a pipe extrusion grade high density polyethylene copolymer offering an excellent combination of stiffness and stress crack resistance. This material meets or exceeds.. |
|||
Melt Flow | 0.25 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® HE3490-LS Black High Density Polyethylene for Pressure Pipes Borstar HE3490-LS is a black, bimodal, high density polyethylene classified as an MRS 10.0 material (PE100) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding.. |